Description: TIPPLEN K 793 is a high molecular weight impact copolymer polypropylene for extrusion. The grade offers excellent processability and impact strength. Applications: TIPPLEN K 793 is recommended for corrugated cardboards, corrugated pipes, sheets, films and blow molded bottles. (1) Average mechanical property values of several measurements carried out on standard injection-molded test specimens prepared in accordance with ISO 294-1. Information provided by Molgroup Chemicals |