I-series (Ionomer): E-FLEX Ionomer is a family of ethylene acrylic acid (E/AA) copolymers, in which part of the acrylic acid is neutralized with metal ions such as zinc (Zn) or sodium (Na) or magnesium (Mg). E-FLEX Ionomer resins deliver impact toughness, abrasion resistance and chemical resistance in a variety of consumer and industrial products. E-FLEX Ionomer can be used in packaging, molded consumer goods, sports goods, and polymer modification. Information Provided by E-Polymers Co., Ltd. |