MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Reynolds EZ~Spray® 45 Sprayable Urethane Rubber Compound
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: EZ~Spray® 45 is a polyurethane rubber for spraying through the EZ~Spray® Junior Cartridge System. Refer to EZ~Spray® Junior manual prior to spraying this product. EZ~Spray® 45 can be sprayed onto vertical surfaces for making molds or is good for making fast molds of large surface areas. After a suitable thickness is attained, EZ~Spray® 45 cures overnight with negligible shrinkage to a durable mold rubber. Application of a support shell is achieved by spraying Smooth-On’s EZ~Spray® Plastic over the rubber mold after it has fully cured. EZ~Spray® 45 is suitable for casting a variety of materials including wax, gypsum, urethane or epoxy resins, concrete, etc.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.025 g/cc1.025 g/ccASTM D-1475
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545ASTM D-2240
Tensile Strength 3.52 MPa510 psiASTM D-412
Elongation at Break 375 %375 %ASTM D-412
Tear Strength 17.5 kN/m100 pliDie C; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 960 min16.0 hour
Pot Life 20.0 min20.0 minASTM D-2471
 
Descriptive Properties
ColorLight Blue
Mix Ratio1A:1Bby volume
Mixed ViscositySprayable
Specific Volume27[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN088 / 296789

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.