MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Starex® SD-0160 Super High Impact Grade ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Water Absorption 0.30 %ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cmASTM D955
Melt Flow 13 g/10 min
@Load 10.0 kg,
Temperature 220 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 98ASTM D785
Tensile Strength, Yield 5700 psi
@Thickness 3.17 mm
ASTM D638
Elongation at Break 87 %
@Thickness 3.17 mm
ASTM D638
Flexural Strength 8700 psi
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 280000 psi
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 8.10 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 180 °F
@Thickness 6.35 mm
Unannealed; ASTM D648
Vicat Softening Point 96.0 °CUnannealed; ISO R 306
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Optical PropertiesOriginal ValueComments
Gloss 96 %ASTM D523
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 374 - 410 °F
Middle Barrel Temperature 392 - 428 °F
Front Barrel Temperature 410 - 446 °F
Melt Temperature 428 - 464 °F
Mold Temperature 104 - 176 °F
Drying Temperature 176 - 185 °F
Dry Time 2 - 4 hour
Injection Pressure 9950 - 15600 psi
Back Pressure 100 - 200 psi
Screw Speed 60 - 80 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-765A ABS - Flame Retardant
BASF Neopolen® P 92HD 105 Expanded Polypropylene (Europe)
Overview of materials for Polypropylene, Flame Retardant
Lotte Advanced Materials Starex® WX-9130 ASA
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded

PLBST002 / 50484

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.