MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Cabot CAB-O-SILĀ® TS-620 Fumed Silica
Categories: Other Engineering Material

Material Notes: Product highlights: CAB-O-SIL TS-620 fumed silica is a medium surface area fumed silica which has been surface modified with dimethyldichlorosilane. The treatment replaces some of the hydroxyls on the surface of the silica, resulting in increased hydrophobicity and very different performance than untreated silica. CAB-O-SIL TS-620 fumed silicas is characterized by:
  • High purity
  • Aggregated structure
  • Submicron particle size
  • Low bulk density
  • Hydrophobic surface chemistry
Key applications: CAB-O-SIL TS-620 fumed silica is used primarily for rheology control in non-polar to medium polarity inks, coatings, silicones and adhesives. CAB-O-SIL TS-620 fumed silica can be an effective thickener in non-polar to medium polarity systems. Although its thickening potential is lower than that of an untreated fumed silica of equal base surface area, the different thixotropic response of CAB-O-SIL TS-620 fumed silica can provide better flow and leveling, resulting in better surface appearance for final products. In moisture-sensitive systems such as urethanes and silicones, the hydrophobic surface of CAB-O-SIL TS-620 fumed silica introduces less moisture than an untreated silica of comparable base surface area typically does. The benefits of decreased moisture are reduction in the amount of moisture scavengers and increased storage stability for the formulation. The surface chemistry of CAB-O-SIL TS-620 fumed silica is more compatible with non-polar systems than untreated silica, allowing for easier incorporation and better dispersion.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT098 / 315833

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.