MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ineos Nova N5000MG Compact PS  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: General purpose polystyrene Microgranulates, having a diameter of 0.5-0.7 mm, providing a very large specific surface area, especially designed for extrusion applications like film, foamed boards and profiles. These products will have an optimal combination of dimensional stability, mechanical properties and high heat resistance.

Information provided by NOVA Chemicals.

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³DIN 53479
Water Absorption <= 0.10 %<= 0.10 %24 hr; DIN 53495
Melt Flow 2.5 g/10 min2.5 g/10 minDIN 5375/ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 55.0 MPa7980 psiSingle stage pre-expansion in continuous expander at atmospheric pressure; DIN 53455
 105 MPa15200 psiDIN 53542/ ISO 178
Elongation at Break 3.5 %3.5 %Single stage pre-expansion in continuous expander at atmospheric pressure; DIN 53455
 5.0 %5.0 %DIN 53542/ ISO 178
Modulus of Elasticity 3.30 GPa479 ksiSingle stage pre-expansion in continuous expander at atmospheric pressure; DIN 53457
Flexural Modulus 2.90 GPa421 ksiDIN 53457/ ISO 178
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²Single stage pre-expansion in continuous expander at atmospheric pressure; DIN 53453/ ISO 179
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²Single stage pre-expansion in continuous expander at atmospheric pressure; DIN 53453/ ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.160 W/m-K1.11 BTU-in/hr-ft²-°FDIN 52612
Vicat Softening Point 100 °C212 °FDIN 53460

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Edistir N 2380 Polystyrene
INEOS Styrolution Polystyrol 168 N GR 2 PS
INEOS Styrolution 153F Polystyrene
CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam
BASF Pluracol® 1026 Molded Foam Polyol

PNOVA314 / 55212

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.