Description: Aluminum and copper foil tapes offer high conformability, conductivity, and reflectivity at elevated temperatures. Aluminum is available with a fiberglass laminate for applications requiring higher tear strengths. Service temperatures range from -100°F to +500°F (-73°C to +260°C). Applications include thermal spray, aircraft repainting, EMI/RFI shielding, and electroplating. All data based on a 0.0035 inch test sample.(Thickness given is for both backing and adhesive. Backing thickness is .0035 inches.) Information provided by Saint Gobain Performance Products. |