MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe LSS™ 135M Nitriding Steel (ASTM A355 Class A)
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: TLS 135M Nitriding Steel is a high-aluminum and chromium modification of AISI 4140 alloy steel. The aluminum addition promotes the formation of aluminum nitride compounds when tools manufactured from this steel are surface nitrided. The result is a nitrided surface which exhibits high hardness and good resistance to abrasion and wear, along with a strong and tough inner core in the piece. TLS 135M is supplied in the prehardened condition at a hardness of approximately 28 to 32 Rockwell C. In this condition, tools can be machined or ground, and then nitrided. Additional heat treatment is normally not required. Typical applications for TLS 135M steel include injection and extrusion feed screws, machine parts, pump parts, bushings, shafts, pinions, crankshafts, cams, camshafts, gears, valve sleeves, chuck jaws, dowel pins, and thread guides.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.86 g/cc
Density 0.284 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 225 inches; Mid-Radius
 273 inches; Mid-Radius
 305 inches; Surface
 303 inches; Surface
 30Up to 1.5 inches; Un-Nitrided
Tensile Strength, Ultimate 112 ksi5 inches; Un-Nitrided
 125 ksi3 inches; Un-Nitrided
 140 ksiUp to 1.5 inches; Un-Nitrided
Tensile Strength, Yield 655 MPa5 inches; Un-Nitrided
 689 MPa3 inches; Un-Nitrided
 827 MPaUp to 1.5 inches; Un-Nitrided
Modulus of Elasticity 30000 ksi
Machinability 70 - 75 %1% Carbon Steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.68 µm/m-°C
@Temperature 0.000 - 500 °C
Thermal Conductivity 360 BTU-in/hr-ft²-°F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 1.15 %
Carbon, C 0.40 %
Chromium, Cr 1.6 %
Iron, Fe 95.6 %
Manganese, Mn 0.60 %
Molybdenum, Mo 0.35 %
Silicon, Si 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Crucible Steel Nitriding #135 Modified Steel, AISI 4140 Modified
Latrobe Nitralloy® 135 Modified VAC-ARC, 1.5 to 3 in Premium Nitriding Steel
Latrobe LSS™ 4140 Alloy Steel (AISI 4140)
Latrobe LSS™ 4142 Alloy Steel (AISI 4142)
Latrobe Nitralloy® 135 Modified VAC-ARC, 3 to 5 in Premium Nitriding Steel

NTIMK124 / 19471

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.