MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Synplast™ TINTM-E Triisononyl Trimellitate
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Branched C9 trimellitate ester

Contains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidant

Information provided by PolyOne; Geon® Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.971 - 0.981 g/cc
@Temperature 25.0 °C
ASTM D4052
Kinematic Viscosity 330 cSt
@Temperature 25.0 °C
ASTM D445
Kinematic Viscosity at 40°C (104°F) 126 cSt
@Temperature 40.0 °C
ASTM D445
Kinematic Viscosity at 100°C (212°F) 11.9 cSt
@Temperature 100 °C
ASTM D445
Molecular Weight 589 g/molTheoretical
ASTM Color 100Pt-Co Scale, Maximum; ASTM D1209
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.020wt% as TMA; ASTM D1045
 
Thermal PropertiesOriginal ValueComments
Pour Point -40.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.48
@Temperature 25.0 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %ASTM D1533
 
Descriptive Properties
AppearanceClear, cleanASTM D2090
 Clear/Transparent
Ester Content99%ASTM D3465; Minimum
FormsLiquid
Generic MaterialTriisononyl Trimellitate
Generic NameTriisononyl Trimellitate
Processing MethodCompounding
Regional AvailabilityAsia Pacific
 Europe
 North America
 South America
UsesCable Jacketing
 Insulation
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Palatinol® N Diisononyl Phthalate
The Chemical Company VESTINOL® 9 Diisononyl Phthalate, C6H4(COOC9H19)2
Teknor Apex TruVis Esters™ TIDTM Tri-Isodecyl Trimellitate

PH0POL0938 / 145507

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.