MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Saint-Gobain CHR® 2300-5R UHMW Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape

Material Notes: CHR® 2300 is manufactured from UHMW (Ultra High Molecular Weight) polyolefin film coated with rubber adhesive.

Features/Benefits: CHR® 2300 exhibits excellent abrasion resistance and it has a low coefficient of friction, making it an excellent protection for surfaces or bearings that experience heavy wear. CHR® 2300 is more economical than PTFE tapes. The high-temperature, high-tack rubber adhesive adheres readily to most dry, clean surfaces, firmly anchoring the product in place.

Applications: 2300 tapes can be used to provide an abrasion-resistant, anti-stick, anti-friction surface at temperatures up to 107 °C. CHR® 2300 is frequently used to line chutes and conveyors. CHR® 2300 is often applied to guide rails to reduce noise levels in glass bottling plants. This tape is also used to replace desk drawer bearings to provide silky smooth, friction-free drawer movement.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 350 %350 %
Coefficient of Friction 0.11 - 0.250.11 - 0.25Kinetic
Tear Strength 7.01 kN/m40.0 pliInitial Tear Strength
Peel Strength 0.600 kN/m3.42 pliAdhesion to Steel
Taber Abrasion, mg/1000 Cycles <= 0.40
@Load 0.100 kg
<= 0.40
@Load 0.221 lb
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 107 °C225 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTGQZ369 / 68883

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.