MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite North America FM 3001 Cellulose Reinforced Phenolic Novolac
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Cellulose Filled

Material Notes: FM 3001 is a self-lubricated cellulose reinforced phenolic molding compound, modified for applications requiring reduced friction and low wear.

Information supplied by Sumitomo Bakelite North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.450 g/ccPowder; ASTM D1895
Density 1.41 g/ccASTM D-792
Water Absorption 0.60 %24 hour; ASTM D570
 1.2 %48 hour; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 115ASTM D785
Tensile Strength, Ultimate 42.0 MPaASTM D638
Flexural Strength 60.0 MPaASTM D790
Flexural Modulus 7.60 GPaASTM D790
Compressive Strength 160 MPaASTM D695
Izod Impact, Notched 0.320 J/cmASTM D256A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 24.0 µm/m-°C
@Temperature 20.0 °C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 180 °CAs Molded; ASTM D648A
 
Descriptive Properties
Available Molding GradesCompression, Transfer, Injection
ColorBlack
FormGranular

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics MACOR® Mac-MGCW Technical Ceramic
Bakelite® UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Bakelite® UP 3720 Unsaturated Polyester Resin, UL Listed, Low Shrinkage, High Arc Resistance
Bakelite® UP 3420 Unsaturated Polyester Resin, High Mechanical Strength, High Arc Resistance, UL Listed, Low Shrinkage
Bakelite® PF 6510 Phenolic Molding Compound

P90XR21 / 21235

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.