MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen HP3644 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Moplen HP3644 is a polypropylene homopolymer designed for the production of biaxially oriented polypropylene films (BOPP). The product is suitable for metallizable film, use in monolayer and in coextruded structures. It contains a standard processing stabilization but does not contain any slip, antiblocking agents and is Calcium Stearate free. Moplen HP3644 offers good optical, easy processing and very good film profile. Typical applications are BOPP packaging films and Solid Phase Thermoforming sheets. Moplen HP3644 is suitable for food contact

Status: Developmental

Availability: Africa-Middle East; Europe

Application: Food Packaging Film; Thermoformed Food Containers

Market: Consumer Flexible Packaging

Processing Method: BOPP; Thermoforming

Attribute: Good Processability; High Clarity; High Gloss; Homopolymer; Medium Flow

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183-1
Melt Flow 3.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70.0ISO 868
Tensile Strength at Break 23.0 MPa50 mm/min; ISO 527-1, -2
Tensile Strength, Yield 33.0 MPaASTM D638
 34.0 MPa50 mm/min; ISO 527-1, -2
Elongation at Break >= 500 %ISO 527-1, -2
Elongation at Yield 11.0 %ASTM D638
 12.0 %50 mm/min; ISO 527-1, -2
Flexural Modulus 1500 MPaASTM D790
Izod Impact, Notched 34.0 J/m
@Temperature 34.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °CUnannealed; ISO 75B-1, -2
 97.0 °CASTM D648
Vicat Softening Point 154 °CA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9692 / 324627

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.