MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Parker Chomerics Tecknit CON/RTV-II 2 Part Silver Filled RTV
Categories: Polymer; Adhesive

Material Notes: Description: TECKNIT electrically conductive, medium viscosity adhesive- sealant system. It is formulated with a special conductive material producing its own unique advantages. After full cure, the resultant bond or seal of the material is flexible, resilient and conductive.

Application Information: TECKNIT Conductive Adhesive-Sealants are recommended wherever an electrically conductive flexible bond and seal is required. The main consideration for selecting the correct adhesive should be based on the galvanic coupling of metallic (or conductive) materials. Excellent practices and recommendations can be obtained by reviewing MIL-STD- 1250. The Adhesive-Sealants are also used to join and install a variety of conductive elastomers and porous or open wire mesh gaskets.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 0.414 MPa>= 60.0 psiCured; ASTM D1002
Peel Strength >= 0.526 kN/m>= 3.00 pliSilicone Aluminum; Cured; ASTM D1876
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.010 ohm-cm<= 0.010 ohm-cmCured; QAP-1017
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °FCured
Minimum Service Temperature, Air -55.0 °C-67.0 °FCured
Shrinkage <= 31 %<= 31 %Cured
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min168 hour
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
followed by 24 hr @ 100°C
Pot Life 4.0 min
@Temperature 25.0 °C
4.0 min
@Temperature 77.0 °F
Shelf Life 9.00 Month9.00 MonthUnopened Container
 
Descriptive Properties
ColorBeige
ConsistencyPaste
FillerAG/Glass
Final ConditionFlexible
Mix Ratio49:1
Number of ComponentsTwo
ResinSilicone
Volume13.6 in3
Weight16 oz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME399 / 131109

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.