MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Michelman® Michem® Emulsion 52137 Nonionic polyethylene emulsion
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Nonionic polyethylene emulsion

Usage: Michem® Emulsion 52137 as an additive, provides lubricity and is effective as a high temperature mold release for metal dies.

We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foam

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 - 1.00 g/cc0.980 - 1.00 g/cc
Volatiles 62.5 - 63.5 %62.5 - 63.5 %
pH 2.0 - 122.0 - 12Recommended pH of system
 8.5 - 9.58.5 - 9.5
Brookfield Viscosity <= 100 cP<= 100 cPSpindle # 2, rpm 60
 
Descriptive Properties
AppearanceLight yellow, translucent liquid
Emulsifier ChargeNonionic
Solids TypePolyethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Michelman® Michem® Emulsion 93235 Nonionic polyethylene emulsion
Michelman® Michem® Emulsion 47950 Nonionic paraffin emulsion
Michelman® Michem® Emulsion 45745P Nonionic Polyethylene wax emulsion
Michelman® Michem® Emulsion 32535 Nonionic, polyethylene emulsion
Michelman® Michem® Emulsion 29730 Nonionic polyethylene emulsion

WMICHEL090 / 135007

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.