MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Primef® 5084 30% GF PPS, Lubricated Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled

Material Notes: Contains PTFE lubricant. Used for injection molding of high performance parts.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/inSolvay Test Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 140 MPa20300 psiISO 527
Elongation at Break 1.8 %1.8 %ISO 527
Tensile Modulus 12.0 GPa1740 ksiISO 527
Flexural Strength 190 MPa27600 psiISO 178
Flexural Modulus 10.5 GPa1520 ksiISO 178
Izod Impact, Notched 0.550 J/cm1.03 ft-lb/inISO 180
Izod Impact, Unnotched 4.00 J/cm7.49 ft-lb/inISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FISO 75
Glass Transition Temp, Tg 90.0 °C194 °F
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 320 - 350 °C608 - 662 °F
Melt Temperature 320 - 330 °C608 - 626 °F
Mold Temperature 150 - 160 °C302 - 320 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 1301/GF/30/TF/15 PPS, linear with glass fiber and PTFE
RTP Company RTP 1300 TFE 30 Polyphenylene Sulfide (PPS), PTFE Lubricated
RTP Company RTP 1303 TFE 10 Polyphenylene Sulfide (PPS), Glass Fiber Reinforced - PTFE Lubricated
RTP Company RTP 1305 C TFE 15 Polyphenylene Sulfide (PPS); Glass Fiber Reinforced - PTFE Lubricated
RTP Company RTP 1305 TFE 13 SI 2 Polyphenylene Sulfide (PPS), Glass Fiber Reinforced - PTFE & Silicone Lubricated

PSOL8Z224 / 101378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.