MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M 2205 Thin Flexographic Plate Mounting Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Thin Flexographic Mounting Tape 2205 is a double coated film tape constructed of a polyester film carrier with differential adhesives specifically designed for the corrugated printing business to hold flexographic print plates to PVC saddles/carriers. Both adhesives are designed to provide high holding power and to cleanly remove from both the plate and the carrier. This product uses the 3M proprietary Easy Mount liner, which creates micro-channels in the linered side adhesive surface. The crosshatched pattern creates a continuous and permanent network of micro-channels in the adhesive, allowing air to escape from between the tape and the carrier.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 4.00 milPaper Liner
 5.00 milTape
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 1.875 pliInitial, Non-linered side-Photopolymer; ASTM D3330
 2.1875 pliLinered Initial, Stainless Steel; ASTM D3330
 2.8125 pliInitial, Linered side-PVC; ASTM D3330
 2.8125 pliNon-Linered Initial, Stainless Steel; ASTM D3330
 4.0625 pli24 hr, Non-linered side-Photopolymer; ASTM D3330
 4.6875 pli72 hr, Non-linered side-Photopolymer; ASTM D3330
 7.50 pli24 hr, Linered side-PVC; ASTM D3330
 7.8125 pli72 hr, Linered side-PVC; ASTM D3330
 
Descriptive Properties
LinerPolyester

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik SAF 2205 Plate, Sheet and Coil

PMM33954 / 168701

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.