MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Thermx® CG933 NC010 PCT
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced

Material Notes: Thermx® CG933 NC010 is a 30% glass reinforced, flame retardant polycyclohexylenedimethylene terephthalate resin for injection molding.

Celenese acquired the Thermx product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.63 g/ccASTM D 792
Density 1.63 g/ccISO 1183
Filler Content 30 %
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 2.00 mm
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.00 mm
ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 114 MPaISO 527
Tensile Strength, Ultimate 120 MPa
@Temperature 23.0 °C
ASTM D 638
Elongation at Break 1.5 %ISO 527
 2.0 %
@Temperature 23.0 °C
ASTM D 638
Tensile Modulus 10800 MPa
@Temperature 23.0 °C
ISO 527
Flexural Strength 172 MPaISO 178
 180 MPaASTM D 790
Flexural Modulus 9600 MPaASTM D 790
 10000 MPaISO 178
Izod Impact, Notched 0.900 J/cm
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 690 J/m
@Temperature 23.0 °C
ASTM D 4812
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 3.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D 257
Surface Resistance 1.00e+16 ohmASTM D 257
Dielectric Constant 3.0
@Frequency 10000 Hz,
Temperature 23.0 °C
ASTM D 150
 3.0
@Frequency 100000 Hz,
Temperature 23.0 °C
ASTM D 150
 3.0
@Frequency 1e+6 Hz,
Temperature 23.0 °C
ASTM D 150
 3.1
@Frequency 1000 Hz,
Temperature 23.0 °C
ASTM D 150
Dielectric Strength 20.4 kV/mm
@Thickness 3.20 mm,
Temperature 23.0 °C
500 V/s, Short Time; ASTM D149
Dissipation Factor 0.0020
@Frequency 100000 Hz
ASTM D 150
 0.0090
@Frequency 1e+6 Hz
ASTM D 150
 0.011
@Frequency 10000 Hz
ASTM D 150
 0.014
@Frequency 1000 Hz
ASTM D 150
Comparative Tracking Index 440 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 285 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 276 °CASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75-1/-2
 255 °CASTM D 648
UL RTI, Electrical 150 °C
@Thickness 1.50 mm
UL 746B
 150 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical without Impact 150 °C
@Thickness 1.50 mm
UL 746B
 150 °C
@Thickness 3.00 mm
UL 746B
Flammability, UL94 V-2
@Thickness 0.790 mm
IEC 60695-11-10
 V-2
@Thickness 0.790 mm
UL94
 V-0
@Thickness 1.50 mm
UL94
 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
UL94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 300 °COptimum
 295 - 310 °C
Mold Temperature 100 °COptimum
 80.0 - 120 °C
Drying Temperature 95.0 °C
Dry Time 4 - 6 hourDehumidified Dryer
Moisture Content <= 0.030 %
 
Descriptive Properties
ColorBlack
Drying RecommendedYes
FeaturesElectrical Properties, Good
 Flame Retardant
FillerGlass fiber reinforcement
FormsPellets
GenericPCT
Part Marking Code>PCT-GF30FR(17)<ISO 11469
Polymer FamilyPolyester
Polymer TypePCT
Processing MethodInjection Molding
Product CategoryElectrical Resins
 Flame Retardant Resins
 Glass Reinforced Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationPCT-GF30FR(17)ISO 1043
UsesConnectors
 E/E Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® HTN51G35HSL NC010 PA6T/XT-GF35
Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
Celanese Zenite® 6130 BK010 LCP, 30% glass reinforced (Extended Tabular Temperature Data)
Celanese VECTRA C130 LCP, 30% Glass Reinforced

PDTA7734 / 89693

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.