General Notes on Meldin 3000/5000 Series Bearing Products: Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water. Specific Notes on Meldin®3000A Bearing Meldin® 3000A is an excellent, multi-purpose wear resistant material that is suitable for bearing, thrust washer and piston ring applications. Meldin® 300A requires a minimum mating surface hardness of Rockwell C35. Information provided by Saint Gobain Performance Products. |