MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 97065 General Purpose Aluminum Foil Tape
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Polymer; Tape

Material Notes: 60 lb. moisture stable liner. Good for die-cut applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 45.7 microns1.80 milBacking; ASTM D3652
 82.5 microns3.25 milTotal; ASTM D3652
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 31.9 MPa4630 psiASTM D3759
Peel Strength 0.438 kN/m2.50 pliAdhesion to Steel; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -34.0 °C-29.2 °F
 
Descriptive Properties
Adhesive TypeAcrylic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 1450 Aluminum Foil Tape
Haynes Hastelloy® W alloy as a weld filler, base metal Type 304 Stainless steel 12.7 mm plate weldments
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy
3M 425 Premium Performance Aluminum Foil Tape
3M 425 Aluminum Foil Tape

PMM34413 / 169160

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.