MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 4500 TFE 20 Aliphatic Polyketone (PK); PTFE Lubricated - Preliminary Datasheet
Categories: Polymer; Thermoplastic; Polyketone

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D 792
Additive Loading 20 %20 %Primary Additive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.3 MPa7000 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 1.59 GPa230 ksiASTM D 638
Flexural Strength 51.7 MPa7500 psiASTM D 790
Flexural Modulus 1.65 GPa240 ksiASTM D 790
Izod Impact, Notched 0.801 J/cm
@Thickness 3.20 mm
1.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 17.1 J/cm
@Thickness 3.20 mm
32.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Processing PropertiesMetricEnglishComments
Melt Temperature 232 - 271 °C450 - 520 °F
Mold Temperature 51.7 - 98.9 °C125 - 210 °F
Drying Temperature 79.4 °C
@Time 14400 sec
175 °F
@Time 4.00 hour
Moisture Content <= 0.10 %<= 0.10 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.250" thick)
RTP Company RTP 4500 TFE 10 Aliphatic Polyketone, PTFE 10%
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Chemours Teflon® PTFE 7A Granular Molding Powder
Chemours Teflon® NXT 75 Fluoropolymer Resin Modified PTFE Granular Molding Resin

PQZRA38675 / 205871

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.