MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Abarco (Albarco) Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Test material of Colombian origin

Key Words: Cariana pyriformis; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.480 g/ccGreen, Central/South American Origin
Density 0.521 - 0.601 g/ccat nominal specific gravity
 0.580 - 0.681 g/ccat oven-dry state
 0.608 - 0.718 g/ccat 9.3% m.c.
 0.666 g/ccNominal; at 9.3% m.c.
Moisture Absorption at Equilibrium 1.5 - 2.0 %Between 40% RH and 90% RH
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 4500 NSide Hardness, 12% Moisture, Central/South American Origin
Modulus of Rupture 0.100 GPaStatic Bending, 12% Moisture, Central/South American Origin
Flexural Modulus 10300 MPaStatic Bending, 12% Moisture, Central/South American Origin
Compressive Strength 47.0 MPaParallel to Grain, 12% Moisture, Central/South American Origin
Shear Strength 15.9 MPaParallel to Grain, 12% Moisture, Central/South American Origin
Work to Maximum Load 0.0950 J/cm³Static Bending, 12% Moisture, Central/South American Origin
 
Thermal PropertiesOriginal ValueComments
Shrinkage 2.8 %Radial Shrinkage Green to Oven Dry, Central/South American Origin
 5.4 %Tangential Shrinkage Green to Oven Dry, African Origin
 9.0 %Volumetric Shrinkage Green to Oven Dry, Central/South American Origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
African Mahogany Wood
Afrormosia Wood
Alerce Wood
American Andiroba Wood
American Ash Wood

PTSM000 / 71353

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.