MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
GEM Brass, Copper Alloy, UNS C49260, H04 Temper, Rod, Bar & Wire
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: Hard

Good Suitability – Soldering, Brazing; Fair Suitability – Capacity for Being Cold Worked, Capacity for Being Hot Formed

Typical Uses: Electric and electronic parts; Environmentally friendly Faucets and Plumbing Components

Applicable Specifications: Forgings, Die (Hot Pressed) – ASME SB283, ASTM B283/B283M; Rod, Bar & Shapes – Forgings ASTM B124/B124M; Rod, Bar & Wire – Free-Cutting ASTM B974/B974M, ASTM B967/B967M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.301 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 67.0 ksi
Tensile Strength, Yield >= 45.0 ksi0.2% Offset
Elongation at Break >= 3.0 %
Tensile Modulus 15800 ksi
Modulus of Rigidity 5600 ksi
Poissons Ratio 0.41Calculated
Machinability 90 %
Forgeability 70 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000790 ohm-cm21.7% IACS
Magnetic Permeability 1.58
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.33 µin/in-°F
@Temperature 20.0 - 100 °C
 9.00 µin/in-°F
@Temperature 20.0 - 200 °C
 10.1 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 45.5 BTU-in/hr-ft²-°F
Melting Point 1623 - 1670 °F
Solidus 1623 °F
Liquidus 1670 °F
Annealing Point >= 932 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= 572 °FStress Relief
Hot-Working Temperature >= 1328 °F
 
Component Elements PropertiesOriginal ValueComments
Bismuth, Bi 0.50 - 1.8 %
Cadmium, Cd <= 0.0010 %
Copper, Cu 58 - 63 %
Iron, Fe <= 0.50 %
Lead, Pb <= 0.090 %
Phosphorus, P 0.050 - 0.15 %
Silicon, Si <= 0.10 %
Tin, Sn <= 0.50 %
Zinc, Zn 34.4 - 41.5 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC49260x6 / 292071

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.