MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.912 - 0.955 g/cc0.0329 - 0.0345 lb/in³Average value: 0.922 g/cc Grade Count:75
Environmental Stress Crack Resistance 5.00 - 1000 hour5.00 - 1000 hourAverage value: 209 hour Grade Count:5
Thickness 31.8 - 50.8 microns1.25 - 2.00 milAverage value: 34.5 microns Grade Count:5
Melt Flow 0.160 - 20.0 g/10 min0.160 - 20.0 g/10 minAverage value: 1.65 g/10 min Grade Count:76
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 45.0 - 59.045.0 - 59.0Average value: 50.3 Grade Count:27
Tensile Strength, Ultimate 10.3 - 18.0 MPa1500 - 2610 psiAverage value: 13.8 MPa Grade Count:25
Film Tensile Strength at Yield, MD 9.38 - 25.5 MPa1360 - 3700 psiAverage value: 14.8 MPa Grade Count:8
Film Tensile Strength at Yield, TD 9.31 - 21.4 MPa1350 - 3100 psiAverage value: 13.3 MPa Grade Count:9
Tensile Strength, Yield 8.48 - 26.2 MPa1230 - 3800 psiAverage value: 12.7 MPa Grade Count:27
Film Elongation at Break, MD 100 - 1070 %100 - 1070 %Average value: 316 % Grade Count:30
Film Elongation at Break, TD 450 - 1340 %450 - 1340 %Average value: 642 % Grade Count:30
Elongation at Break 80.0 - 920 %80.0 - 920 %Average value: 534 % Grade Count:31
Elongation at Yield 11.0 - 640 %11.0 - 640 %Average value: 334 % Grade Count:3
Modulus of Elasticity 0.150 - 0.520 GPa21.8 - 75.4 ksiAverage value: 0.300 GPa Grade Count:16
Flexural Modulus 0.152 - 2.21 GPa22.0 - 320 ksiAverage value: 0.327 GPa Grade Count:25
Secant Modulus, MD 0.130 - 0.214 GPa18.9 - 31.0 ksiAverage value: 0.181 GPa Grade Count:24
Secant Modulus, TD 0.160 - 0.591 GPa23.2 - 85.7 ksiAverage value: 0.223 GPa Grade Count:23
Elmendorf Tear Strength MD 150 - 780 g150 - 780 gAverage value: 327 g Grade Count:16
Elmendorf Tear Strength TD 100 - 1820 g100 - 1820 gAverage value: 306 g Grade Count:28
Dart Drop 2.20 - 4.72 g/micron56.0 - 120 g/milAverage value: 3.31 g/micron Grade Count:4
Dart Drop Test 60.0 - 1300 g0.132 - 2.87 lbAverage value: 161 g Grade Count:28
Film Tensile Strength at Break, MD 15.0 - 40.0 MPa2180 - 5800 psiAverage value: 25.3 MPa Grade Count:28
Film Tensile Strength at Break, TD 15.0 - 45.0 MPa2180 - 6530 psiAverage value: 20.4 MPa Grade Count:26
 
Thermal PropertiesMetricEnglishComments
Melting Point 108 - 121 °C226 - 250 °FAverage value: 113 °C Grade Count:12
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 54.0 °C104 - 129 °FAverage value: 47.0 °C Grade Count:7
Vicat Softening Point 85.0 - 111 °C185 - 232 °FAverage value: 94.6 °C Grade Count:39
Brittleness Temperature -76.1 - 0.500 °C-105 - 32.9 °FAverage value: -70.5 °C Grade Count:15
 
Optical PropertiesMetricEnglishComments
Haze 3.40 - 22.0 %3.40 - 22.0 %Average value: 8.51 % Grade Count:27
Gloss 20.0 - 120 %20.0 - 120 %Average value: 70.8 % Grade Count:16
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 225 °C302 - 437 °FAverage value: 187 °C Grade Count:4
Melt Temperature 110 - 260 °C230 - 500 °FAverage value: 190 °C Grade Count:14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Overview of materials for Low Density Polyethylene (LDPE), Sheet/Profile extrusions

O3806 / 78250

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.