MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chambroad Petrochemicals Electret Masterbatch
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Functional Masterbatch: The electret masterbatch is made from polypropylene with special additives uniformly dispersed in the masterbatch. It can increase the charge trapping density in the melt-blown nonwoven fabric, reduce the resistance with the same fiber fineness and gram weight, and improve the overall filtration efficiency of the nonwoven fabric. It is mainly suitable for high-efficiency electret treatment of melt-blown fabrics in the melt-blowing industry.

Information provided by Shandong Chambroad Petrochemicals Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.20 %<= 0.20 %Method A in GB/T 2914-2008
Melt Flow 1000 - 1700 g/10 min1000 - 1700 g/10 minMethod B in GB/T 3682-2000 Method B
Ash 1.7 - 2.7 %1.7 - 2.7 %Method A in GB/T 9345.1-2008
 
Descriptive Properties
Granule appearanceBig granules and small granules<20g/kg, SH/T1541-2006
 Black granule0 piece/kg, SH/T1541-2006

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAMB022 / 318564

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.