MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Specialty Materials 5521 Boron Epoxy Prepreg Tape
Categories: Polymer; Thermoset; Epoxy

Material Notes: Specialty Materials' 5521 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, 250°F curing epoxy resin. Performing at temperatures up to 350°F, 5521 tape is an economical solution for composite structure fabrication. It is a 2-step tape in various widths produced from initial ¼-inch width tape stock.

Information provided by Specialty Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/cc
Thickness 130 micronscured ply
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1520 MPa
Elongation at Yield 0.80 %
Modulus of Elasticity 185 GPa
Flexural Yield Strength 1790 MPa
Flexural Modulus 190 GPa
Compressive Yield Strength 2930 MPa
Compressive Modulus 210 GPa
Poissons Ratio 0.21
Shear Modulus 6.30 GPa
Shear Strength 97.0 MPaInterlaminar
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 177 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 121 °CCure Temp.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 977-6 Epoxy Laminate with IM7 Unidirectional Tape
Specialty Materials Hy-Bor 208 Boron/Graphite Hybrid Prepreg Tape
Fibre Glast 3100 Style 7781 Prepreg E-Glass Fiberglass Fabric
Arlon Electronic Materials 44N Multifunctional Microdispersed Ceramic Filled Epoxy-Fiberglass Prepreg
Solvay CYCOM® 381 Epoxy E-glass Prepreg

PSPEC00 / 68529

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.