MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

(Viewing data as-entered. Click here to return)
INEOS Styrolution NAS® 90 Styrene Methyl Methacrylate (SMMA)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Styrene/Methyl Methacrylate Copolymer (SMMA)

Material Notes: NAS® 90 is a styrene acrylic copolymer that can be used in a variety of applications demanding a strong, stiff water-clear plastic resin with excellent thermal stability. Sparkling clarity, Low density, Ease of processing, Gamma & ETO sterilizable, Meets USP XXIII specifications for Class VI plastics, UL 94 HB approved

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccISO 1183
Moisture Absorption at Equilibrium 0.10 %
@Temperature 23.0 °C
50% RH; ISO 62
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmISO 294-4
Melt Flow 16 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 65
Ball Indentation Hardness 168 MPaISO 2039-1
Tensile Strength, Yield 60.0 MPaISO 527
Elongation at Break 2.3 %ISO 527
Tensile Modulus 3100 MPaISO 527
Flexural Strength 100 MPaISO 178
Flexural Modulus 3200 MPaISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²ISO 180
 2.50 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 13.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °Cannealed; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 90.0 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 97.0 °C
@Load 1.02 kg
B/2 120C/H; ASTM D 1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.56Sodium D Line; ISO 489
Haze 0.30 %ASTM D 1003
Transmission, Visible 91 %
@Wavelength 550 nm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 180 - 210 °C
Middle Barrel Temperature 200 - 230 °C
Front Barrel Temperature 210 - 240 °C
Melt Temperature 200 - 240 °CISO 294
Mold Temperature 30.0 - 60.0 °CISO 294
Drying Temperature 80.0 °C
@Time 7200 sec
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Injection VelocitySlow to ModerateISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution NAS® 30 Styrene Methyl Methacrylate (SMMA)
INEOS Styrolution NAS® 21 Styrene Methyl Methacrylate (SMMA)
INEOS Styrolution NAS® 36 Styrene Methyl Methacrylate (SMMA)
Denka TX-100S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene

PSTYR9863 / 216090

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.