- ISO 7391-PC,MP,(,,)-09-9
- MVR (300 °C/1.2 kg) 6.0 cm3/10 min
- Impact modified
- High viscosity
- Injection molding - Melt temperature 280 - 320 °C
- Available in opaque colors only