MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Carpenter Pyrotough® 78 Hot Work Die Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Tool Steel; Hot Work Steel

Material Notes: Pyrotough® 78 alloy is a premium quality hot work die steel engineered to withstand the operating temperatures and pressures associated with die casting and hot extrusion operations. The patented composition of the alloy displays improved temper resistance/red-hardness and similar toughness when compared to standard AISI type H13 hot work die steel. Careful control over all stages of processing results in an alloy possessing a high degree of purity, homogeneity and microstructural integrity.

Applications: mandrels for extruding copper, brass, stainless steel, and nickel-base superalloys, dies for extruding copper and brass

Information provided by Carpenter Technology Corporation.

Pyrotough® is a registered trademark of Carpenter Technology Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.75 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 54As hardened
 56.5Tempered at 1000°F
Tensile Strength, Ultimate 1860 MPa3 in bar
 1515 MPa
@Temperature 427 °C
3 in bar
Tensile Strength, Yield 1655 MPa
@Strain 0.2 %
3 in bar
 1480 MPa
@Strain 0.2 %,
Temperature 427 °C
3 in bar
Elongation at Break 9.0 %Elongation in 4D, 3 in bar
 15 %
@Temperature 427 °C
Elongation in 4D, 3 in bar
Reduction of Area 43 %3 in bar
 59 %
@Temperature 427 °C
3 in bar
Charpy Impact 14.9 JV Notch, 3 in bar
 29.8 J
@Diameter 3.00 mm,
Temperature 427 °C
V-Notch, bar
Abrasion 120loss in mm3, Tempered at 1025°F; ASTM G65
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.6 µm/m-°C
@Temperature 27.0 - 600 °C
Transformation Temperature 857 °CAc1
 913 °CAc3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 %
Chromium, Cr 4.45 %
Iron, Fe 90.845 - 90.85 %As Balance
Manganese, Mn 0.45 %
Molybdenum, Mo 2.05 %
Silicon, Si 1.0 %
Sulfur, S <= 0.0050 %
Vanadium, V 0.80 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
420 Stainless Steel
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel
AISI Type H13 Hot Work Tool Steel
Cast Stainless Steel CA15B
MetalTek MTEK CA20NW Cast UNS J91631 Martensitic Stainless Steel

NCARN14 / 15853

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.