MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Taiwan PU RPU-26-16C Moisture Reactive Hot Melt Adhesive for WR Fabric 4 Grade
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Key features:
  • 100% solid content
  • Good chemical resistance & hydrolysis resistance
  • Great yellowing resistance
  • High bonding performance & temperature resistance
  • Solvent-free Eco-friendly
Application: This grade is moisture reactive hot melt adhesive. It can be applied on the lamination of textile, textile/TPU film…etc.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Viscosity  1100 cP
@Temperature 130 °C
1100 cP
@Temperature 266 °F
 4000 cP
@Temperature 100 °C
4000 cP
@Temperature 212 °F
 15000 cP
@Temperature 80.0 °C
15000 cP
@Temperature 176 °F
Brookfield Viscosity 3250 - 3800 cP
@Temperature 105 °C
3250 - 3800 cP
@Temperature 221 °F
DV-II +,Sp.27, 50RPM
 
Descriptive Properties
AppearanceSemi-yellowish, half transparent and half solid form (at room temperature)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTAIWPU129 / 305859

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.