MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem AKROCHEM® Peptizers 4P
Categories: Other Engineering Material

Material Notes: Product Description: Peptizers 4P and 6P are activated 2,2'-dibenzamido diphenyldisulfide (DBDD) absorbed on a clay carrier. These products are used as processing aids/viscosity reducers for natural and synthetic rubbers.

Applications: Peptizers 4P and 6P are effective chemical peptizers primarily used for natural rubber. Recommended dosage levels in natural rubber are 0.05 to 0.50 phr (as final mixing temperature increases, the lower levels should be used). Synthetic rubbers require approximately 2.0 phr. By promoting chain scission during mastication, compound viscosities and dump temperatures are lowered. Also, processing, mold flow and uniformity of extruded stocks are improved. DBDD has very little effect on physical properties of vulcanizates and is acceptable per FDA CFR 21 177.2600. Peptizer 4P and 6P disperse readily in rubber and should be added at the beginning of the mixing cycle, using either internal mixers or open mills. Viscosity reduction is most effective when the rubber and peptizer are premasticated before adding other ingredients. It is possible to eliminate the premastication step in internal mixers, where temperatures exceed 212°F/100°C, by adding carbon black, zinc oxide, stearic acid, and oils after the Peptizer 4P/6P addition. It is important, however, that sulfur, antioxidants, retarders and accelerators be added at the end of the mix cycle since they will interfere with peptization. For styrene butadiene (SBR) it is recommended not to exceed 266oF processing temperatures to prevent possible cyclization reactions. If higher than recommended levels of Peptizer 4P/6P are used, be sure antioxidant is present in the compound to prevent unfavorable aging of vulcanizates. These products, especially Peptizer 6P, have a blueish cast and can discolor light-colored stocks (white, tans, yellows).

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/cc
Ash 45 %
 
Descriptive Properties
Appearancegrayish powder
Content0.45Active DBDD

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH551 / 315469

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.