MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro Bayhydrol® UH 240 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Aliphatic anionic polyester polyurethane dispersion. As a combination binder in the formulation of highly flexible, water-thinnable, air- and force-drying primers and one-coat finishes for use on plastics.

Properties / Applications: Bayhydrol® UH 240 can be used in combination with hydrofunctional resins, preferably Bayhydrol® U XP 2698, Bayhydrol® U 2757 and Bayhydrol® U 355 either Bayhydrol® U 475, in the formulation of highly flexible two-component polyurethane top coats (e.g. in soft-feel coating systems). After crosslinking with, e.g. Bayhydur® 3100 force-drying (e.g. 30 - 45 min at 80 °C) yields films with good surface handle and good resistance to abrasion and water.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccDIN EN ISO 2811-2
Volatiles 59 - 61 %59 - 61 %1g/1h/125°C; DIN EN ISO 3251
Particle Size <= 210 µm<= 210 µm
pH 6.0 - 8.06.0 - 8.0DIN ISO 976
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.500.50[mg KOH/g]; DIN EN ISO 2114
 
Descriptive Properties
Appearancemilky, cloudy

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0171 / 201954

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.