MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
American Black Ash (Brown Ash) Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Ring-Porous Hardwood

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Fraxinus nigra; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.530 g/ccOven-dry to green volume ratio
Density 0.460 g/ccOven Dry Weight/Unseasoned Volume
 53.0 lb/ft³Unseasoned*
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 2400 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2600 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 490 psiPerpendicular to Grain*
Modulus of Elasticity 11.04 GPaASTM D143 at 12 wt% moisture content
Modulus of Rupture 0.08797 GPaASTM D143 at 12 wt% moisture content
 6.00 ksiStatic Bending*
Flexural Yield Strength 2600 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 1020 ksiStatic Bending*
Compressive Strength 430 psiPerpendicular to Grain*
 1620 psiParallel to Grain*
 2290 psiMax Crushing Strength Parallel to Grain*
Shear Strength 870 psiParallel to Grain*
Impact 2.5in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 7200psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.420 in-lb/in³Static Bending*
Work to Maximum Load 12.4 in-lb/in³Static Bending*
Cleavage 46.0 kN/mTangential surface of failure, Unseasoned*
 48.0 kN/mRadial surface of failure, Unseasoned*
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.150 W/m-KASTM D143 at 12 wt% moisture content
Shrinkage 5.0 %Radial; Unseasoned to Oven Dry*
 7.8 %Tangential; Unseasoned to Oven Dry*
 14.4 %Volumetric; Unseasoned to Oven Dry*

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Red Maple Wood
American Chestnut Wood
American Ash Wood
American Black Gum (Black Tupelo) Wood
Silver Maple (Water Maple, White Maple), Soft Wood

PTSA000 / 71238

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.