MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Braskem INSPIRE™ 117 Performance Polypropylene Polymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade; Polypropylene, Extrusion Grade

Material Notes: D 117.00 Developmental Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistance, and clarity are required.

  • Outstanding heat resistance
  • Excellent balance of high stiffness and toughness
  • Good contact clarity and gloss
  • Low taste and odor transfer
  • Contains a nucleating agent
  • Complies with U.S. FDA 21 CFR 117.1520(c)

This product line was spun off from Dow Chemical to Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Index of Compound 2.1 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 33.8 MPaASTM D638
Elongation at Yield 5.0 %ASTM D638
Flexural Modulus, 1% Secant 1720 MPaASTM D790A
Izod Impact, Notched 560 J/mASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 116 °CUnannealed; ASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem INSPIRE™ 404 Performance Polypropylene Polymer
Dow INSPIRE™ 117.00 Performance Polymer
Dow INSPIRE™ 404 Performance Polymer
Braskem INSPIRE™ 222 Performance Polypropylene Polymer
Braskem INSPIRE™ 114 Performance Polypropylene Polymer

PDOW0995 / 93331

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.