MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Styrene/Methyl Methacrylate Copolymer (SMMA)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 - 1.13 g/cc0.0329 - 0.0408 lb/in³Average value: 1.07 g/cc Grade Count:31
Water Absorption 0.0900 - 1.00 %0.0900 - 1.00 %Average value: 0.196 % Grade Count:12
Moisture Absorption at Equilibrium 0.100 - 0.150 %0.100 - 0.150 %Average value: 0.130 % Grade Count:5
Linear Mold Shrinkage 0.00200 - 0.00700 cm/cm0.00200 - 0.00700 in/inAverage value: 0.00405 cm/cm Grade Count:20
Melt Flow 0.400 - 30.0 g/10 min0.400 - 30.0 g/10 minAverage value: 7.01 g/10 min Grade Count:31
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 65.0 - 85.065.0 - 85.0Average value: 74.8 Grade Count:10
Hardness, Shore D 69.0 - 75.069.0 - 75.0Average value: 72.0 Grade Count:4
Ball Indentation Hardness 168 - 169 MPa24400 - 24500 psiAverage value: 169 MPa Grade Count:4
Tensile Strength, Ultimate 21.0 - 65.5 MPa3050 - 9500 psiAverage value: 41.5 MPa Grade Count:20
Tensile Strength, Yield 14.0 - 85.0 MPa2030 - 12300 psiAverage value: 50.1 MPa Grade Count:20
Elongation at Break 2.00 - 280 %2.00 - 280 %Average value: 31.0 % Grade Count:30
Elongation at Yield 1.00 - 3.00 %1.00 - 3.00 %Average value: 2.00 % Grade Count:9
Modulus of Elasticity 0.820 - 3.45 GPa119 - 501 ksiAverage value: 2.68 GPa Grade Count:21
Flexural Yield Strength 88.0 - 113 MPa12800 - 16400 psiAverage value: 99.4 MPa Grade Count:9
Flexural Modulus 1.58 - 3.40 GPa229 - 493 ksiAverage value: 2.79 GPa Grade Count:19
Izod Impact, Notched 0.160 - 5.55 J/cm0.300 - 10.4 ft-lb/inAverage value: 0.506 J/cm Grade Count:21
Izod Impact, Unnotched 1.76 - 100 J/cm3.30 - 187 ft-lb/inAverage value: 2.11 J/cm Grade Count:9
Izod Impact, Notched (ISO) 2.00 - 14.0 kJ/m²0.952 - 6.66 ft-lb/in²Average value: 6.50 kJ/m² Grade Count:6
 2.70 - 2.70 kJ/m²
@Temperature -30.0 - -30.0 °C
1.28 - 1.28 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 2.70 kJ/m² Grade Count:1
Charpy Impact Unnotched 1.20 - 2.04 J/cm²5.71 - 9.69 ft-lb/in²Average value: 1.49 J/cm² Grade Count:6
Charpy Impact, Notched 0.141 - 0.200 J/cm²0.670 - 0.952 ft-lb/in²Average value: 0.168 J/cm² Grade Count:8
 0.200 - 0.200 J/cm²
@Temperature -30.0 - -30.0 °C
0.952 - 0.952 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.200 J/cm² Grade Count:1
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °FAverage value: 260 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 76.0 - 100 °C169 - 212 °FAverage value: 86.1 °C Grade Count:13
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 98.9 °C140 - 210 °FAverage value: 82.3 °C Grade Count:22
Vicat Softening Point 85.0 - 106 °C185 - 223 °FAverage value: 99.0 °C Grade Count:29
Flammability, UL94 HBHBGrade Count:6
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.54 - 1.571.54 - 1.57Average value: 1.56 Grade Count:8
Haze 0.200 - 5.00 %0.200 - 5.00 %Average value: 1.65 % Grade Count:18
Transmission, Visible 80.0 - 93.0 %80.0 - 93.0 %Average value: 89.7 % Grade Count:26
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 250 °C374 - 482 °FAverage value: 247 °C Grade Count:10
Melt Temperature 170 - 243 °C338 - 470 °FAverage value: 199 °C Grade Count:14
Mold Temperature 30.0 - 70.0 °C86.0 - 158 °FAverage value: 46.9 °C Grade Count:6
Drying Temperature 70.0 - 82.2 °C158 - 180 °FAverage value: 79.5 °C Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6063-O
Magnesium Elektron Elektron® W15 Magnesium Alloy Welding Rod Composition
Magnesium AZ31B-F, Extruded Solid Shapes
Overview of materials for Styrene Acrylonitrile (SAN), Transparent
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene

O4985a / 89101

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.