MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Plastics Group Polifil® RP-PP Polypropylene, Molding Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Polifil® RP-PP reprocessed polypropylene has the highest stiffness of the commodity olefin resins, while retaining sufficient impact properties for many applications. Due to its low cost and low density, polypropylene use has been expanding rapidly, and common uses now include injection molded articles, fibers, packaging films, and extruded sheet and profiles. Polypropylene is widely used in injection molding for housewares, appliances, and automotive parts. High flow grades are spun into fibers, and molded into thin wall containers, cups, and lids. Moderate flow resins are common in general injection molding and cast films. High molecular weight, low flow grades are extruded into sheet and profiles, and blow molded into automotive parts and recreational goods.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792
Density 0.905 g/cc0.0327 lb/in³ASTM D792
Water Absorption 0.00 %0.00 %24 hours; ASTM D570
Linear Mold Shrinkage 0.0200 cm/cm
@Thickness 3.17 mm
0.0200 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 10 - 20 g/10 min10 - 20 g/10 min230/2.16; May be specified; ASTM D1238
 0.900 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.900 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70.070.0ASTM D1415
Tensile Strength 31.0 MPa4500 psiASTM D638
Tensile Strength, Yield 29.0 MPa4200 psiASTM D638
Elongation at Break 20 %20 %ASTM D638
 50.0 %50.0 %ASTM D638
Elongation at Yield 11.0 %11.0 %ASTM D638
Tensile Modulus 1.38 GPa200 ksiASTM D638
Flexural Strength 41.4 MPa6000 psiASTM D790
Flexural Modulus 0.124 GPa18.0 ksitangent; ASTM D790
Flexural Modulus, 1% Secant 1240 MPa180000 psiASTM D790
Izod Impact, Notched 0.267 J/cm0.500 ft-lb/inASTM D256
 0.320 J/cm0.600 ft-lb/inASTM D256
Izod Impact, Unnotched 6.41 J/cm12.0 ft-lb/inASTM D256
Gardner Impact 2.71 J
@Thickness 12.7 mm
2.00 ft-lb
@Thickness 0.500 in
tup; ASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C200 °FASTM D648
 96.1 °C205 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C120 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Molded
Chase Plastics CP Pryme® PE100-LD2M General Purpose Low Density Polyethylene
Braskem PH 1721 HOMO Polypropylene Homopolymer
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene
Borealis Borpact™ SG910MO Polypropylene for Injection Molding

PPOLI058 / 56962

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.