MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Adflex Q 190 F Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Adflex Q 190 F is a thermoplastic polyolefin, which is mainly used by our customers for the extrusion of blown film. It is also suitable for sheet extrusion. Adflex Q 190 F features very high softness and very low modulus. It does not contain any slip or anti-blocking agents. Adflex Q 190 F is used for the production of soft hygienic film and heavy duty film, as well as for the modification of LDPE or LLDPE to increase mechanical characteristics, puncture resistance, and to allow further down gauging. It can be easily processed on conventional LDPE or LLDPE blown film lines.

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America

Application: Agriculture Film; Bags & Pouches; Barrier Film; Breathable Film; Collapsible Tubes; Film Wrap; Food Packaging Film; Heavy Duty Packaging; Hygiene Film; Interior Automotive Applications; Lamination Film; Shrink Film; Stretch Hood; Surface Protection Film; TPO Foils and Skins

Market: Flexible Packaging; Rigid Packaging

Processing Method: Blown Film; Calendaring; Double Bubble; Extrusion Blow Molding; Extrusion Flat-die; Sheet; Thermoforming

Attribute: Good Flexibility; Good Processability; Good Puncture Resistance; Good Tear Strength; Low Temperature Impact Resistance; Low Transparency; Soft

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³ISO 1183-1
Melt Flow 0.600 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.600 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 30.0
@Time 15.0 sec
30.0
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 10.0 MPa1450 psiISO 527-1, -2
Elongation at Break 400 %400 %ISO 527-1, -2
Flexural Modulus 0.100 GPa14.5 ksiISO 178
Charpy Impact, Notched  0.500 J/cm²
@Temperature -40.0 °C
2.38 ft-lb/in²
@Temperature -40.0 °F
ISO 179
 11.0 J/cm²
@Temperature -20.0 °C
52.3 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 142 °C288 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 40.0 °C104 °FUnannealed; ISO 75B-1, -2
Vicat Softening Point 60.0 °C140 °FA/50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9006 / 323934

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.