MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Hapco ULTRALLOY 306 Polyurethane Liquid, Flame Retardant
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: A series of clear, flame retardant (UL94 V-O), Liquid Molding Compounds. This series has an ultimate hardness of 85D and tensile strengths from 8,900 psi to 10,600 psi are available.:
  • 1:1 by weight
  • Flame retardant, meets UL 94V-0
  • Clear/translucent when cured

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D-4669
Viscosity 225 - 325 cPASTM D-4878
Linear Mold Shrinkage 0.0010 - 0.0030 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ASTM D-2240
Tensile Strength 8900 psiASTM D-638
Elongation at Break 14.4 %ASTM D-638
Modulus of Elasticity 197 ksiASTM D-638
Flexural Strength 13200 psiASTM D-790
Flexural Modulus 352 ksiASTM D-790
Izod Impact, Notched 0.660 ft-lb/inASTM D-256
Izod Impact, Unnotched >= 9.40 ft-lb/inASTM D-256
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 60.0 °CASTM D-648
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 8.00 hour
@Thickness 3.17 mm
Demold
Gel Time 25.0 min
@Load 0.100 kg
ASTM D-2971
 
Descriptive Properties
Color (cured)clear / hazy
Mix Ratio100:100Weight
 100:107Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHAPCO188 / 317247

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.