MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotchkote™ GP 120 Epoxy Primer
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Primer GP 120 has been specifically developed as an anti corrosive coating for steel structures that cannot be abrasive blast cleaned.

Product Features:

  • Suitable for use on mechanically prepared steelwork or high pressure water cleaned steel, can also be used on abrasive blasted steel.
  • Can be applied over existing coatings.
  • Can be used as a two coat primer/finish system or overcoated with a variety of top coats.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³
Solids Content 90 %90 %
Volatile Organic Compounds (VOC) Content 83 g/l83 g/l
Thickness 3180 microns125 milDry
 3560 microns140 milWet
 
Processing PropertiesMetricEnglishComments
Cure Time 360 min6.00 hourTouch Dry
 1440 min24.0 hourHard Dry
 10100 min168 hourFull Cure
 
Descriptive Properties
AppearanceSilver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35290 / 170037

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.