MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Beijing Chemical Industry KAIFA® GL1100 ABS General Purpose Grade
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: High gloss, excellent external appearance

Information provided by Beijing Chemical Industry Research Institute (Group)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D792
Water Absorption 0.30 %24 hr; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 53.0 MPaASTM D638
Elongation at Break 20 %ASTM D638
Flexural Strength 85.0 MPaASTM D790
Flexural Modulus 2.40 GPaASTM D790
Izod Impact, Notched 18.0 J/m
@Thickness 3.20 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °CASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 230 °CResin Temp.
Rear Barrel Temperature 190 °C
Middle Barrel Temperature 210 °C
Front Barrel Temperature 220 °C
Nozzle Temperature 215 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 - 90.0 °C
@Thickness 30.0 mm
Dry Time 4 hour
@Thickness 30.0 mm
Injection Pressure 80.0 - 130 MPainjection speed: 80 - 120 rpm
Back Pressure 1.00 - 2.00 MPaMold Pressure
Screw Speed 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Edinburg Plastics AGG625 ABS
Ineos ABS Lustran® 1465, Injection Grade
IRPC Polimaxx Porene GA300 Acrylonitrile Butadiene Styrene
LG Chemical HI121U ABS
LG Chemical XR407D ABS

PKAIF61 / 48643

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.