MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic stability compared to other polyester based TPUs. Its typical applications seals, gaskets, belting, hose jacketing, tubing, animal ID tags and other fabricated products.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Thickness 1.59 mm
plaque
Linear Mold Shrinkage, Transverse 0.0060 - 0.0070 cm/cm
@Thickness 1.59 mm
plaque
Melt Flow 29 g/10 min
@Load 1.20 kg,
Temperature 224 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90 - 98ASTM D2240
Hardness, Shore D 54 - 62ASTM D2240
Tensile Strength at Break 42.0 MPa
Elongation at Break 540 %
50% Modulus 0.00841 GPa
@Strain 50 %
100% Modulus 0.0103 GPa
@Strain 100 %
300% Modulus 0.0207 GPa
@Strain 300 %
Flexural Modulus 0.0758 GPa
Tear Strength 131 kN/m
Taber Abrasion, mg/1000 Cycles 10H22 Wheel
Compression Set 30 %
@Temperature 23.0 °C
 40 %
@Temperature 70.0 °C
Tensile Set 60 %Elongation set after break
 
Thermal PropertiesOriginal ValueComments
CTE, linear 151 µm/m-°C
@Temperature 20.0 °C
Vicat Softening Point 89.0 °C
Glass Transition Temp, Tg -24.0 °C
Clash Berg Stiffness Temperature -39.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 193 - 210 °COptimum Extrusion Temperature
Melt Temperature 213 - 216 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Tecoflex® EG-93A TPU - Clear
Dow Pellethane® 2102-90AR Polyurethane Elastomer, Polyester Polycaprolactone Based
Dow ISONATE™ 125M Pure MDI
Dow Pellethane® 2102-85A Polyurethane Elastomer, Polyester Polycaprolactone Based
Dow Pellethane® 2354-45D Polyurethane Elastomer, Polyester Polycaprolactone Based

PDW262 / 34430

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.