MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon 32400R040 0.040" (1.02 mm) Uncured Silicone Rubber on PET Carrier
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Design/Construction:
Side 1: Uncured Silicone Rubber
Carrier: PET
Interleave: Polyethylene

Appearance: Red silicone rubber on polymer liner

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccSilicone Property; Arlon SQA-TMS-024
Thickness 3.00 milInterleave
 5.00 milCarrier
 40.0 milOverall; Arlon SQA-TMS-003
 40.0 milSide 1; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55Silicone Property; ASTM D2240
Tensile Strength 1083 psiSilicone Property; ASTM D412
 1187 psiPost Cured Product; ASTM D412
Elongation at Break 711 %Silicone Property; ASTM D412
 718 %Post Cured Product; ASTM D412
Tear Strength 248 pliSilicone Compound; ASTM D624
 273 pliPost Cured Product; ASTM D624
Compression Set 9.0 %Post Cured Product, Silicone Property; ASTM D395
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 807 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -70.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 227 °C
Recommended Postcure Cycle, after 30 minute ramp up cycle
 30.0 min
@Temperature 177 °C
Recommended Cure Cycle
Shelf Life 3.00 Month
@Temperature 21.1 °C
From date of manufacture
 
Descriptive Properties
ColorRed
Total Product Weight (oz/yd2)38Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow C6-350LH ELASTOMER KIT
Dow C6-180 ELASTOMER KIT
Dow 5-8601 FLUOROSILICONE LSR, KIT
Dow 3-6891 1-PART SILICONE RUBBER ABRADABLE SEALANT COMPOUND
Dow 3-6655 THERMALLY CONDUCTIVE ELASTOMER, KIT

PARL173 / 125359

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.