MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Nylatron® 4.6 (ASTM Product Data Sheet)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Unreinforced

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Water Absorption 0.60 %Immersion, 24hr; ASTM D570
Water Absorption at Saturation 7.0 %ASTM D 570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 97ASTM D785
Tensile Strength 15000 psiASTM D638
Tensile Strength at 150°C (300°F) 250 psiASTM D638
Tensile Strength at 65°C (150°F) 6000 psiASTM D638
Elongation at Break 25 %ASTM D638
Tensile Modulus 470 ksiASTM D638
Flexural Strength 17000 psiASTM D790
Flexural Modulus 450 ksiASTM D790
Compressive Strength 16000 psi10% Def.; ASTM D695
Compressive Modulus 325000 psiASTM D695
Izod Impact, Notched 0.600 ft-lb/inASTM D256
K (wear) Factor 100 x 10-10 in³-min/ft-lb-hrQTM 55100
Limiting Pressure Velocity 2700 psi-ft/minQTM 55007
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+13 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µin/in-°F
@Temperature -40.0 - 150 °C
ASTM E831
Thermal Conductivity 2.10 BTU-in/hr-ft²-°F
Melting Point 554 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 300 °FContinuous
Deflection Temperature at 1.8 MPa (264 psi) 320 °FASTM D648
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA No
NSF No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Limited
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Limited
Conductive / Static Dissipative No
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron™ GSM PA6 Nylon, Cast MoS2 Filled Type 6
Mitsubishi Chemical Advanced Materials Nylatron™ 703 XL PA6 Cast, Wear Resistant, Zero 'Stick-Slip
Mitsubishi Chemical Advanced Materials Nylatron™ MC 901 H.S. PA6
Mitsubishi Chemical Advanced Materials Nylatron™ SLG-FDA PA6
Mitsubishi Chemical Advanced Materials Nylatron™ GSM Blue PA6 Cast Oil & MoS2 Filled Type 6

P1SM25D / 89257

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.