MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gougeon Brothers PRO-SET® LAM-135/LAM-239 Laminating Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Medium viscosity for good wet out of all synthetic composite fabrics and core materials.
Extended open timer hardener provides 8 to 9 hours of working time at 85°F (29°C). A typical laminate will be gelled in 12 to 14 hours at 85°F (29°C).
Optimized for hand wet out and machine impregnation in contact molding, vacuum bagging and filament winding applications.
Elevated temperature cure is required; thermal and mechanical properties suitable for composite components and high-temperature tooling and molds.
Tg as high as 215°F (102°C) with proper post cure providing excellent temperature stability and great part cosmetics.
Cost effective, high performance epoxy formulation for synthetic composite manufacturing.
Quality-control tinting is available at no extra charge; simply add "QC" after the product code on your order.

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccHardener
 1.16 g/ccCured
 1.16 g/ccResin
Viscosity 116 cP
@Temperature 22.0 °C
hardener; ASTM D2196
 250 cP
@Temperature 48.9 °C
Mixed
 1000 cP
@Temperature 29.4 °C
Mixed
 1085 cP
@Temperature 29.0 °C
Mixed; ASTM D2196
 1544 cP
@Temperature 25.0 °C
Mixed; ASTM D2196
 1976 cP
@Temperature 22.0 °C
Mixed; ASTM D2196
 2900 cP
@Temperature 15.6 °C
Mixed
 6890 cP
@Temperature 22.0 °C
resin; ASTM D2196
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D2240
 86
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D2240
 91
@Treatment Temp. 60.0 °C,
Time 57600 sec
RT Gelation; ASTM D2240
Tensile Strength 10200 psi
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D638
 10200 psi
@Treatment Temp. 60.0 °C,
Time 57600 sec
RT Gelation; ASTM D638
 10300 psi
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D638
Elongation at Break 4.8 %
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D638
 6.2 %
@Treatment Temp. 60.0 °C,
Time 57600 sec
RT Gelation; ASTM D638
 6.3 %
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D638
Tensile Modulus 405000 psiRT Gelation; ASTM D638
 458000 psiRT Gelation; ASTM D638
 483000 psiRT Gelation; ASTM D638
Flexural Strength 17700 psi
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D790
 17700 psi
@Treatment Temp. 60.0 °C,
Time 57600 sec
RT Gelation; ASTM D790
 17700 psi
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D790
Flexural Modulus 421000 psi
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D790
 484000 psi
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D790
 484000 psi
@Treatment Temp. 60.0 °C,
Time 57600 sec
RT Gelation; ASTM D790
Compressive Yield Strength 14100 psi
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D695
 14100 psi
@Treatment Temp. 60.0 °C,
Time 57600 sec
RT Gelation; ASTM D695
 14100 psi
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D695
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 162 °F
@Treatment Temp. 60.0 °C,
Time 28800 sec
RT Gelation; ASTM D648
 174 °F
@Treatment Temp. 60.0 °C,
Time 57600 sec
RT Gelation; ASTM D648
 208 °F
@Treatment Temp. 82.0 °C,
Time 28800 sec
RT Gelation; ASTM D648
Glass Transition Temp, Tg 221 °FASTM E1356
 167 °F
@Treatment Temp. 60.0 °C,
Time 28800 sec
DSC Onset– 1st Heat, RT Gelation, 1 Hz, 3°C per minute; ASTM E1356
 169 °F
@Treatment Temp. 60.0 °C,
Time 57600 sec
DSC Onset– 1st Heat, RT Gelation, 1 Hz, 3°C per minute; ASTM E1356
 181 °F
@Treatment Temp. 60.0 °C,
Time 28800 sec
DMA Onset Storage Modulus, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 188 °F
@Treatment Temp. 60.0 °C,
Time 57600 sec
DMA Onset Storage Modulus, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 210 °F
@Treatment Temp. 60.0 °C,
Time 28800 sec
DMA Peak Tan Delta, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 215 °F
@Treatment Temp. 82.0 °C,
Time 28800 sec
DMA Onset Storage Modulus, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 215 °F
@Treatment Temp. 82.0 °C,
Time 28800 sec
DSC Onset– 1st Heat, RT Gelation, 1 Hz, 3°C per minute; ASTM E1356
 219 °F
@Treatment Temp. 60.0 °C,
Time 57600 sec
DMA Peak Tan Delta, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 241 °F
@Treatment Temp. 82.0 °C,
Time 28800 sec
DMA Peak Tan Delta, RT Gelation, 1 Hz, 3°C per minute; ASTM E1640
 
Processing PropertiesOriginal ValueComments
Cure Time 12.0 - 14.0 hour
@Temperature 29.0 °C
typical laminate will be gelled
Pot Life 94.0 - 116 min
@Load 0.500 kg,
Temperature 29.0 °C
ASTM D2471
 123 - 151 min
@Load 0.500 kg,
Temperature 25.0 °C
ASTM D2471
 142 - 194 min
@Load 0.150 kg,
Temperature 29.0 °C
ASTM D2471
 162 - 198 min
@Load 0.500 kg,
Temperature 22.0 °C
ASTM D2471
 187 - 228 min
@Load 0.150 kg,
Temperature 25.0 °C
ASTM D2471
 223 - 272 min
@Load 0.150 kg,
Temperature 22.0 °C
ASTM D2471
Working Life 8.00 - 9.00 hour
@Temperature 29.0 °C
Shelf Life 24.0 Monthhardener
 36.0 Monthresin
 
Descriptive Properties
Mix ratio100:23.4–100:32.5Weight Range, Resin: Hardener
 100:27.9Weight, Resin: Hardener
 100:27.9–100:38.8Volume Range, Resin: Hardener
 100:33.3Volume, Resin: Hardener
 3.00:1Volume, Resin: Hardener
 3.5:1Weight, Resin: Hardener
 3.59:1–2.2.58:1Volume Range, Resin: Hardener
 4.28:1-3.08:1Weight Range, Resin: Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOUGP918 / 290761

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.