MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis HG430MO Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: HG430MO is a polypropylene homopolymer intended for injection molding. This polymer product is characterized by a superior impact resistance. This grade has ductile failure in falling weight impact test at room temperature. This product is characterized by excellent flow properties combined with a narrow molecular weight distribution well suited for low distortion products. This grade contains anti-static and slip additives, which result in short cycle time, good demolding and low dust attraction. Applications: caps and closures, and items requiring good antistatic properties.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 91ISO 2039-2
Tensile Strength, Yield 33.0 MPa50mm/min; ISO 527-2
Elongation at Yield 11 %50mm/min; ISO 527-2
Tensile Modulus 1400 MPa1mm/min; ISO 527-2
Charpy Impact, Notched 3.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Puncture Energy 40.0 JISO 6603-2
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °CISO 75-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °C
Mold Temperature 10.0 - 30.0 °C
Hold Pressure 20.0 - 50.0 MPa
 
Descriptive Properties
Injection Velocityhighest possible

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis RB307MO Polypropylene Random Copolymer
Avient Edgetek® PP-30GF/000 Polypropylene (PP), Glass Filled
A. Schulman PP 3488-01 Polypropylene Homopolymer Polypropylene
Borealis HG313MO Polypropylene
Borealis HF136MO Polypropylene

PBOREA493 / 108752

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.