MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Bayoxide® E 22 Technical Oxide
Categories: Ceramic; Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No: 51274-00-1

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.460 - 0.570 g/cc0.0166 - 0.0206 lb/in³DIN EN ISO 787-11
Loss On Ignition 20 %20 %DIN EN ISO 787-2
Specific Surface Area 120 - 200 m²/g120 - 200 m²/gISO 9277
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Monthbulk bags
 60.0 Month60.0 Monthbags
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.035 %<= 0.035 %<350 mg/kg
Arsenic, As <= 0.0020 %<= 0.0020 %<20 mg/kg
Barium, Ba <= 0.0010 %<= 0.0010 %<10 mg/kg
Cadmium, Cd <= 0.00050 %<= 0.00050 %<5 mg/kg
Chromium, Cr <= 0.025 %<= 0.025 %<250 mg/kg
Cobalt, Co <= 0.010 %<= 0.010 %<100 mg/kg
Copper, Cu <= 0.010 %<= 0.010 %<100 mg/kg
Fe2O3 >= 70 %>= 70 %
Manganese, Mn <= 0.30 %<= 0.30 %<3000 mg/kg
Nickel, Ni <= 0.025 %<= 0.025 %<250 mg/kg
Plutonium, Pu <= 0.00030 %<= 0.00030 %<3 mg/kg
Zinc, Zn <= 0.010 %<= 0.010 %<100 mg/kg
 
Descriptive Properties
Content<1.0%Water soluble content, DIN EN ISO 787-3
Specifications<10%Sieve residue <0.5 mm
 <5%Sieve residue >2.0 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8396 / 208789

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.