MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® LV-5H Nylon 12, 50% Glass Fiber Filled, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 50% Glass Fiber Filled

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Filler/Reinforcement: Glass Fiber, 50% Filler by Weight

Additive: Impact Modifier

Features: Alcohol Resistant; Hydrolysis Resistant; Impact Modified

Uses: Appliance Components; Appliance; Automotive Applications; Automotive Under the Hood; Cell Phones; Connectors; Consumer Applications; Electrical/Electronic Applications; Engineering Parts; Household Goods; Hydraulic Applications; Industrial Applications; Medical Devices; Pneumatic Applications; Power/Other Tools; Sporting Goods

RoSH Compliance: RoSH Compliant

Automotive Specifications: GM GMW15702-022541 PA12-GF50 Color: 9288 Black

Forms: Granules

Processing Method: Injection Molding

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccISO 1183
Water Absorption 0.40 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.80 %ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0010 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 22500 psiISO 527-2
Elongation at Break 5.0 %ISO 527-2
Tensile Modulus 1.74e+6 psiISO 527-1
Charpy Impact Unnotched 43.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eU
 43.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eU
Charpy Impact, Notched 7.10 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 9.00 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 8.30 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 67.0 µin/in-°FISO 11359-2
Melting Point 352 °F10ºC/min; ISO 11357-3
Maximum Service Temperature, Air 194 - 248 °FLong Term; ISO 2578
 302 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 329 °FUnannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 257 °FUnannealed; ISO 75-2/C
Flammability, UL94 HB
@Thickness 0.762 mm
IEC 60695-11-10,-20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGRIM152 / 307511

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.