MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Elastosil® R 752/70 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Vulcanizates made from ELASTOSIL® R 752/70 exhibit a very low rebound resilience and high damping capability.

Application: Some special applications, such as low-modulus damping elements, require silicone rubber with a particularly low impact resilience. ELASTOSIL® R 752/70 meets these requirements.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccDIN 53479
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70DIN 53505
Tensile Strength at Break 9.60 MPaDIN 53504 S1
Elongation at Break 560 %DIN 53504 S1
Rebound 29 %DIN 53512
Tear Strength 27.0 kN/mASTM D624 B
Compression Set 39 %
@Temperature 175 °C,
Time 79200 sec
DIN ISO 815-B
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Treatment Temp. 165 °C
post cured 4h/200°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® R 401/10 Silicone Rubber
SMAC BARRIER® Damping Material
Saint-Gobain COHRlastic® CF4480 High Heat Reversion Resistant Reinforced Solid Rubber
Saint-Gobain COHRlastic® 100S Silicone Sponge/High Temp Silicone Adhesive Pressure Sensitive Tape
Orbilan RubberLen® 70 TPE, light grey

PWACK9233 / 204762

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.