MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Sandvik SAF 3207 HD Tube and pipe, seamless
Categories: Metal; Ferrous Metal; Austenitic; Ferritic; Stainless Steel

Material Notes: Sandvik SAF 3207 HD is a hyper-duplex (austenitic-ferritic) stainless steel for service in highly corrosive conditions where also high mechanical strength is necessary. This makes the grade ideal for applications such as deepwater umbilicals. Sandvik SAF 3207 HD is characterized by:
  • Excellent resistance to pitting and crevice corrosion
  • Excellent resistance to stress corrosion cracking (SCC) in hydrogen sulphide (H S) and chloride containing environments
  • High resistance to general corrosion in acidic and caustic environments
  • Excellent resistance to erosion corrosion
  • Excellent corrosion fatigue properties
  • Exceptionally high mechanical strength
  • Exceptionally high fatigue strength
  • Physical properties that offer design advantages
  • Good weldability

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C <= 36
@Thickness <=4.00 mm
 <= 36
@Thickness >=4.00 mm
Tensile Strength, Ultimate >= 784 MPa
@Temperature 200 °C
 >= 785 MPa
@Temperature 250 °C
 >= 791 MPa
@Temperature 300 °C
 >= 811 MPa
@Temperature 150 °C
 >= 850 MPa
@Temperature 100 °C
 >= 923 MPa
@Temperature 50.0 °C
 >= 850 MPa
@Thickness >=4.00 mm
 >= 950 MPa
@Thickness <=4.00 mm
Tensile Strength, Yield >= 572 MPa
@Strain 0.2 %,
Temperature 300 °C
 >= 582 MPa
@Strain 0.2 %,
Temperature 250 °C
 >= 585 MPa
@Strain 0.2 %,
Temperature 200 °C
 >= 609 MPa
@Strain 0.2 %,
Temperature 150 °C
 >= 657 MPa
@Strain 0.2 %,
Temperature 100 °C
 >= 696 MPa
@Strain 0.2 %,
Temperature 50.0 °C
 >= 700 MPa
@Strain 0.2 %,
Thickness >=4.00 mm
 >= 770 MPa
@Strain 0.2 %,
Thickness <=4.00 mm
Elongation at Break >= 15 %
@Thickness <=4.00 mm
 >= 15 %
@Thickness >=4.00 mm
 >= 25 %
@Thickness <=4.00 mm
Based on L = 5.65 vS where L is the original gauge length and S the original cross section area.
 >= 25 %
@Thickness >=4.00 mm
Based on L = 5.65 vS where L is the original gauge length and S the original cross section area.
Modulus of Elasticity 200 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000870 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.5 µm/m-°C
@Temperature 30.0 - 100 °C
 13.5 µm/m-°C
@Temperature 30.0 - 200 °C
 14.0 µm/m-°C
@Temperature 30.0 - 300 °C
 14.5 µm/m-°C
@Temperature 30.0 - 400 °C
Specific Heat Capacity 0.480 J/g-°C
@Temperature 20.0 °C
 0.510 J/g-°C
@Temperature 100 °C
 0.540 J/g-°C
@Temperature 200 °C
 0.570 J/g-°C
@Temperature 300 °C
 0.590 J/g-°C
@Temperature 400 °C
Thermal Conductivity 13.0 W/m-K
@Temperature 20.0 °C
 15.0 W/m-K
@Temperature 100 °C
 16.0 W/m-K
@Temperature 200 °C
 18.0 W/m-K
@Temperature 300 °C
 20.0 W/m-K
@Temperature 400 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 32 %
Manganese, Mn <= 1.5 %
Molybdenum, Mo 3.5 %
Nickel, Ni 7.0 %
Nitrogen, N 0.50 %
Phosphorus, P <= 0.035 %
Silicon, Si <= 0.80 %
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type S45500 Stainless Steel, hardened at 480°C (900°F) for 4 hours, air cooled
Sandvik SAF 2507 Bar Steel
Outokumpu 4501 Duplex Stainless Steel
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy
AK Steel NITRONIC® 30 Austenitic Stainless Steel

NSANDV5226 / 199790

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.