MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Michelman® Michem® Emulsion 43040 Nonionic polypropylene emulsion
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description: Nonionic polypropylene emulsion

Usage: Michem® Emulsion 43040 is effectively used as an additive in floor polish and overprint varnish formulations when a high degree of slip resistance is needed, as well as a binder lubricant for chopped strand fiberglass

We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foam

Food Contact Information when manufactured in USA and Singapore:
FDA:
175.105: Components of adhesives

Food Contact Information when manufactured in Belgium:
FDA:
175.105: Components of adhesives
176.180: Components of paper and paperboard in contact with dry foods.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.990 - 1.01 g/cc
Volatiles 59.5 - 60.5 %
pH >= 7.0Recommended pH of system
 7.7 - 9.0
Brookfield Viscosity <= 60 cPSpindle # 1, rpm 60
 
Descriptive Properties
AppearanceAmber, translucent liquid
Emulsifier ChargeNonionic
Solids TypeMaleated Polypropylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom HYG 400-2L NAT Polypropylene with 20% Glass Fiber Filler
Spartech EP6430 Filled and Reinforced Copolymer
BYK PRIEX® 25097 Maleic Anhydride Grafted PP random copolymer
BYK PRIEX® 25093 Maleic Anhydride Grafted PP random copolymer
BYK PRIEX® 20097 Maleic Anhydride Grafted PP homopolymer

WMICHEL082 / 134999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.