MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Humiseal 1A33LSE Urethane Conformal Coating
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Humiseal 1A33LSE Urethane Conformal Coating
  • High moisture resistance
  • Excellent dielectrical properties
  • Excellent chemical resistance
  • Repairable
  • UL Approval Pending
  • MIL-I-46058C Approval Pending
  • Passes thermal shock test (MIL-I-46058C)
  • Flammability (self extinguishing) (ASTM D635)
  • Excellent resistance to solvents (IPC CC 830)
  • Recommended Stripper: 1063
  • Recommended Thinner: 801
Cure Type: Heat

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.50 lb/galASTM D1475
Solids Content 50 %Fed Std 141 Method 4044
Volatile Organic Compounds (VOC) Content <= 225 g/l
Viscosity 200 cPFed Std Method 4287
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 3.915 ksi
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.60e+10 ohmMoisture Resistance; MIL-I-46058C
Insulation Resistance 2.00e+14 ohmInsulation Resistance; MIL-I-46058C
Dielectric Constant 3.6ASTM D1 50 65T
Dielectric Breakdown >= 1500 VDielectric Withstand; MIL-I-46058C
Dissipation Factor 0.020ASTM D1 50 65T
 
Thermal PropertiesOriginal ValueComments
CTE, linear 170 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -65.0 °C
Glass Transition Temp, Tg 56.0 °C
Flash Point 60.0 °FASTM D56
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 minDry Time to Handling; Fed Std 141 4061
 10800 - 43200 min
 20.0 hour
@Temperature 190 °C
 30.0 hour
@Temperature 170 °C
Shelf Life 12.0 Month
@Temperature 23.0 °C
 
Descriptive Properties
Coverage375 ft²/gal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMT Materials REN Shape® 450 Prototype Tool & Modeling Board

PHUMIS10 / 47610

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.